SPS spark plasma sintering of W-Re High Specific Gravity Alloy
We prepare the W-Re high specific gravity alloy by SPS spark plasma sintering furnace. The sintering temperature was 1800℃, the sintering pressure was 40MPa, and the holding time was 5min.